Product Description of BGS-385 TIG Welding Wire for Stainless Steel Austenitic Type Compliance: YB/T 5092 H019Cr20Ni25Mo4Cu AWS A5.9 ER385 A5.9M ER385 EN ISO 14343-A: W (20 25 5 Cu L) EN ISO 14343-B: SS385 Purpose Often used for the manufacture of various columns, containers...
BGS-385
TIG Welding Wire for Stainless Steel
Austenitic type
Compliance:
YB/T 5092 H019Cr20Ni25Mo4Cu
AWS A5.9 ER385
A5.9M ER385
EN ISO 14343-A: W (20 25 5 Cu L)
EN ISO 14343-B:SS385
Often used for the manufacture of various columns, containers, pipelines and tanks for storing and transporting strong acids.
1. It is resistant to the general corrosive effects of sulfuric and phosphoric acids, and at atmospheric pressure it is resistant to corrosion in acetic acid of any temperature and concentration;
2. Effectively prevents the problems of intergranular corrosion, pitting corrosion, crevice corrosion and stress corrosion cracking;
3. Stable arc, good weld formation, excellent fluidity of molten metal, excellent welding properties.
| Alloy, wt. % | C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
| YB/T standard | 0.019 | 1.0-2.5 | 0.50 | 19.0-21.5 | 24.0-26.0 | 4.2-5.2 | 0.03 | 0.03 | 1.2-2.0 |
| AWS Standard | 0.019 | 1.0-2.5 | 0.50 | 19.0-21.5 | 24.0-26.0 | 4.2-5.2 | 0.03 | 0.03 | 1.2-2.0 |
| Approximate value | 0.015 | 1.90 | 0.34 | 20.30 | 25.82 | 4.51 | 0.014 | 0.006 | 1.54 |
| Mechanical characteristics | Yield strength, MPa | Tensile strength, MPa | Elongation, % | Impact strength, J/°C | Heat treatment, °C × h |
| YB/T standard | — | — | — | — | — |
| AWS Standard | — | — | — | — | — |
| Approximate value | — | 595 | 38 | 116/-40 | — |
1. Shielding gas: pure argon;
2. Maintain interpass temperature ≤150°C.